Video: Thin Films & Coatings Technology Asia Symposium: Nanoindentation Mapping for Rapid Screening of Stress Corrosion Cracking

Mar 02, 2023

Dr. Janelle Wharry of Purdue University discusses her group’s use of nanoindentation mapping to characterize stress corrosion cracking (SCC) of steel that is used in storing spent nuclear fuel. The research analyzed the nanomechanical properties before and after radiation exposure.