玩偶姐姐

Video: Johann Kappacher: Plastic deformation behavior of Cobalt upon phase transformation revealed by high temperature nanoindentation

Jun 29, 2020

Technically pure cobalt with a phase transformation temperature of 700 K was investigated by high temperature nanoindentation. From the results of constant indentation strain rate experiments as well as strain rate jump tests the rate controlling deformation mechanisms could be derived. For the low temperature hcp phase from room temperature to 450 K a bcc-like deformation behavior was observed, while from 450 K to 700 K it was found that dislocation cross slip bears plasticity. In the high temperature face centered cubic phase cutting of forest dislocations was identified as the dominating deformation mechanism.

Are you sure?

You've selected to view this site translated by Google Translate.
玩偶姐姐 China has the same content with improved translations.

Would you like to visit 玩偶姐姐 China instead?


您已选择查看由骋辞辞驳濒别翻译翻译的此网站。
碍尝础中国的内容与英文网站相同并改进了翻译。

你想访问碍尝础中国吗?

If you are a current 玩偶姐姐 Employee, please apply through the 玩偶姐姐 Intranet on My Access.

Exit