Video: Indentation University Session 22 – Theory of Measuring Stress-Strain Curves by Nanoindentation

Mar 11, 2021

Nanoindentation is a common technique for measuring the Young¡¯s modulus and hardness of metals. With recent advancements, nanoindentation can now be used to measure the entire stress-strain curve, even within a single metal grain. Join Sr. Application Scientist Jennifer Hay for a discussion of the theory behind this new measurement, and how nanoindentation measurements of force, displacement, and stiffness can be interpreted to arrive at the stress-strain curve.