Video: Session 18: How to Prepare Porous 3D-Printed Titanium for Nanoindentation

Sep 25, 2020

Mr. Crawford (former manager of the materials-testing laboratory at Johns Hopkins University) shows how to prepare a porous metal for high-speed nanoindentation. He provides recommendations for equipment and demonstrates all aspects of metallographic mounting and polishing.