Video: Additive Manufacturing Asia Symposium: Nanoindentation Mapping of Metals and Alloys Made by Additive Manufacturing
Professor Yu Zou of the University of Toronto discusses his research in a number of case studies, using nanoindentation techniques to characterize AM-printed materials.