Video: Thin Films & Coatings Technology Symposium: Nanoindentation Mapping for Rapid Screening of Stress Corrosion Cracking


Dr. Janelle Wharry of Purdue University discusses the use of nanoindentation mapping to understand chloride-induced stress corrosion cracking (SCC) mechanisms in cold spray (CS) coatings used as corrosion mitigation barriers. In addition. Dr. Wharry discusses hardness mapping of grains and along cracks induced by stress corrosion.